Hot Melt Glue Stick
OODA ‒ 925S
Product Model:OODA ‒ 925S
Product Color:Milky White
Softening Point:152℃ ± 5℃
Viscosity:180℃ / 14000 ± 1000 CPS
Shape:11mm x 30cm
Ingredients:EVA resin, tackifying resin, paraffin, additives, etc.
Product Features:High bonding strength
Application:Fire resistant. Softening point 150℃. Suit for products need high temperature resistant.
Method of Use:
Insert glue stick inside the glue gun and connect 220V power supply. It can be used after being preheated for ten minutes. The operating temperature is 160℃ ~ 180℃.
Packing and Storage:
Paper bags packing, 25Kg/bag. Stored in a cool and dry place, storage period is two years.
Note:
1. Opening and curing time will vary with the temperature at which the adhesive is heated, coating amount, sticking period and the strength.
2. The temperature of the melting system is high, please do not touch it with your hand in order to avoid scald.
3. If the glue drop on the skin, the burnt part should be immediately immersed in cold water for at least 15 minutes and then sent to hospital to be treated.
OODA ‒ 925S
Product Model:OODA ‒ 925S
Product Color:Milky White
Softening Point:152℃ ± 5℃
Viscosity:180℃ / 14000 ± 1000 CPS
Shape:11mm x 30cm
Ingredients:EVA resin, tackifying resin, paraffin, additives, etc.
Product Features:High bonding strength
Application:Fire resistant. Softening point 150℃. Suit for products need high temperature resistant.
Method of Use:
Insert glue stick inside the glue gun and connect 220V power supply. It can be used after being preheated for ten minutes. The operating temperature is 160℃ ~ 180℃.
Packing and Storage:
Paper bags packing, 25Kg/bag. Stored in a cool and dry place, storage period is two years.
Note:
1. Opening and curing time will vary with the temperature at which the adhesive is heated, coating amount, sticking period and the strength.
2. The temperature of the melting system is high, please do not touch it with your hand in order to avoid scald.
3. If the glue drop on the skin, the burnt part should be immediately immersed in cold water for at least 15 minutes and then sent to hospital to be treated.